Recycling chrome  

September 16, 2008

Is it worth while to strip chrome bumpers (from older cars with large chrome bumpers) to recycle the chrome plating?

Tim Devaney
auto hobbyist - Ridley, PA, USA
contact button


September 23, 2008

Hi, Tim. The thickness of the chrome plating is only several millionths of an inch, and chrome is not a precious metal, being worth only several dollars per pound.

Beneath the chrome, is nickel plating of about .0012" thickness, which is worth something like $7 per pound.

Regards,


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey


Dear reader

Post an answer
 
Post a question
 
Report broken links

 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com