Quick rusting after washing of rotors
September 14, 2008
Presently we wash rotors with Water based chemicals only degreasing-water rinse & passivation But after 24hrs it get rusty? Any neet oil is there for washing of rotors. After washing we are doing Blueing process in furnace.