Painting of 316 SS after passivation

September 16, 2008

I need your help please. Before I even start with painting, I would like to know if I will have any problems applying a P3 coating system onto 316 SS, after pickling and passivation? Does the chemicals have any effect on the coating system??

Pieter van Heerden
quality engineer - Al Jubail, Saudi Arabia
contact button


September 30, 2008

Should not be a problem.