Blisters on zinc plated sheet metal
September 15, 2008
Dear Sir,
we are in sheet metal parts, wherein zinc plating is carried out
simultaniously,
in past 1 year we had a problem of BLISTERING, and this was stopped
due to stabilization of processes, recently we have observed this
problem back.
so could you giude me to do root cause analysis on blister
occurence.
do share with me your experience for such kind of problems.
Kirtikumar Prabhu, Quality Assurance
- Goa, India

September 22, 2008
Hi, Kirtikumar. The single most common cause of blistering would
be inadequate cleaning.
Regards,
|
|

Ted Mooney, P.E.
finishing.com
Brick, New Jersey
|
September 29, 2008
HI SIR,
As Ted Mooney said improper cleaning only leads to blistering
problem. Improve your cleaning process and try.
GOOD LUCK
regards
|
|
Shoban Kesarapu plating chemicals supplier
Secunderabad, A.P., India
|
-
-
 |