We plate Electroless nickel (10%P) on carbon steel substrates. To
improve adhesion and hydrogen release bake them at 200 deg C for 4
hours. Our customer demanded heat treatment under vacuum. Is there
any advantage in going for vacuum? There is no tarnishing of coating
even in normal furnace. Is it really necessary to go for Vacuum? Our
customer says this coating (30 microns) is for corrosion
resistance.For what type of applications baking under vacuum is
needed?
Ram Prasad
job plater - Bangalore, Karnataka, India

September 28, 2008
Conventional furnace may leave surface contamination which in turn
may lead to premature corrosion. Also remember that "The one who
pays, rules". G. Marrufo-Mexico
Guillermo Marrufo
Monterrey, NL, Mexico
-
-
 |