Difference between yellow and white galvanizing?

        

September 21, 2008

hello
I want to know about the diferences between yellow and white galvanizing.
the main thing is that I have fixed the zinc galvanized support with dichromate anchor bolts and sombody rasied the corrosion problem.Is it correct or not?

Mohsen Askari
- Kerman, Iran
  ^- Privately contact this inquirer -^
September 24, 2008

All galvanizing is about the same colour, but it is possible to cause it to have a yellowish colour by chromate passivation. Its the chromate thats yellow, not the galvanizing.

This passivation will keep the zinc looking a bit shinier for longer, but I doubt you'd measure any difference in corrosion protection of the steel underneath.

Mixing passivated with unpassivated galvanizing should present no problems.

Some people comment on dull grey versus shiny silver galvanizing. The difference is due to the reaction between the steel and the zinc. There's no measurable difference in the corrosion proteciton afforded by either.

Geoff Crowley
   galvanizing &
   powder coating shop
Glasgow, Scotland


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search