E-coating material

September 19, 2008

What actually is the material used in the e-coating , which company actually manufactures the genuine e-coating solvent, and what is the minimum thickness of the coating

Milan Patel
R & D head - Gujarat, INDIA
  ^- Privately contact this inquirer -^
September 23, 2008

Hi, Milan. Please describe your own situation and your interest in these issues rather than presenting a dry flash-card quiz :-)

We have found that readers rarely respond to questions that are presented in this fashion. Thanks!

Regards,

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


September 29, 2008

hi sir,
For this infomation I think it is better to consult your local chem supplier.

Shoban Kesarapu
    plating chemicals supplier
Secunderabad, A.P., India


December 4, 2008

Dear Mr Patel,

The material is either water based epoxy or acrylic primer.
PPG, Kanzai, BASF, Dupont are some of the chaps who make the product. The normal thickness applied is around 20 microns thick.

Hope this helps you find whatever you're looking for.

khozema Khozema Vahanwala
Saify Ind
 
Bangalore, Karnataka, India


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search