I need to remove old dark brown paint from aluminum window frames and I've tried the mineral spirits [link is to product info at Amazon], scraping, sanding and the stuff is really stubborn ... any ideas???

Kevin Callan
painter - Gurnee, IL U.S.
contact button


September 22, 2008

Hi, Kevin. aircraft stripper [link is to product info at Amazon] should do it, but it's pretty noxious.

Regards,


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey