Is mixing stainless steel & galvanized hardware compatible for
use on pressure treated lumber? Thank you!
Eddy Oriol
- Wasilla, Alaska USA

September , 2008
Hi, Eddy. They should not touch. You can use stainless for some
stuff and galvanized for other stuff, but you should not be putting
stainless washers on galvanized bolts or vice versa.