50026
Chemical polishing of molds
September 12, 2008
WE ARE DIE CASTING DIE MAKERS, WE WANT TO KNOW IS THERE ANY
PROCESS TO POLISH THE SURFACE OF THE DIE CHEMICALLY OR CHEMICAL
POLISHING. PLEASE SUGGEST.
RAVICHANDRAN
RAVICHANDRAN
DIE MAKER - BANGALORE, KARNATAKA, INDIA

October 8, 2008
There is a new and pattented development from one of the best
known japanese machinery manufacturers that leaves near mirror finish
after EDM. The invention has to do with a special powdery substance
added to the oil. Search "best EDM surface finish" in your favorite
engine.
Guillermo Marrufo
Monterrey, NL, Mexico
-
-
 |