50011

Anti-oxidant material for copper foil  

September 6, 2008

I am student Damascus University I need it for my project

Ayad al-dahhan
student - Damascus
contact button


September 18, 2008

Hi, Ayad. There are a number of ways to deter oxidation of copper, but look into benzotriazole.

Regards,


Ted Mooney, P.E. 