Dear All, I am a PhD student working on titanium implants. i was able to produce porous titanium surface by using 1wt% HF+1M H3PO4.The pore sizes were 300-500 nm. I need pores larger than 2 microns. Could any one please give me any suggestions? Thanks

Toulou Shokuhf
student - Michigan, USA
contact button


October 17, 2008

Try a mixture of 5% KOH + 5% H2O2. It will work slowly, perhaps 4-8 hours @ ambient temp.

Jeffrey Holmes, CEF
- Spartanburg, SC, USA


November 16, 2008

Dear Toulou Shokuhf,

You have to suitably modify the pH, current density and treatment time to modify the pore size.


T.S.N. Sankara Narayanan

- Chennai, Tamilnadu, India


Dear reader

Post an answer
 
Post a question
 
Report broken links

 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com