Need lacquers and lacquer coating machine for buttons and buckles  

September 17, 2008

We have an electroplating plant in which we plate fashion good accessories like buttons, buckles, washers, eyelets, zipper pulls. etc. The size of material to be plated varies from (diameter 1 mm to 10 cm). Our major problem is choice of a correct lacquer and lacquer machine which can apply the lacquer on the objects smoothly and give a pleasent and shiny look.

Our finishes are
antique copper, antique brass, tin, white bronze, antique silver, black nickel free

Can any body select one or more suitable lacquers and methods of application (my major problem is antique silver which becomes yellow even after applying lacquer on it)

Azhar Ali Mahar

Karachi

Azhar Ali Mahar, process Engg
employee - Pakistan
contact button


RFQ button


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com