Material Properties of NarLoy-Z

.

We analyze rocket combustion chambers (such as the Vulcain-Engine of the Ariane Rocket) numerically with a Finite Element Program.

For this purpose, we need to know e.g. a few material properties of NarLoy-Z (such as modulus of elasticity, yield stress, hardening module) in dependence on the temperature. Do you know anyone (or a publication) where we could get this information from? In order to validate our calculation methods, we are going to build a model combustion chamber, possibly from Narloy-Z.

How much is this Material (per kg) and where may we get it from?

J‰rg Richard Riccius
German Aerospace Research Center
DLR - Lampoldshausen, Ba-Wue, Germany


+

I have exactly the same problem that you and I have found out the reference of a publication.

I am trying to get it, so I don't realy know if it is what you are looking for.

I hope it will be useful:

"Journal of Material Science"
Subject: Chemical Sciences
ISSN:022-2461
Volume 32 Issue 14 (1997) pp 3891-3903
Publication Date 01/01/1997 (printed version)
Title: "Mechanical properties and microstructural stability of wrought, laser, and electron beam glazed NARloy-Z alloy at elevated temperatures"

If could foud yet these data by another way, could you please let me know.

Paloma de la PeÒa GarcÌa
- Madrid,Spain

ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search