Black oxidation - nitriding/nitrocarburizing process 

.

I'd like to now more about qpq, or other similar nitriding / nitrocarburizing + black oxidation process.

Which kind of salt is used in the qpq process. What kind of cleaning processes have to be used before nitriding and before oxidation. What environmental problems result from using this salt, in particular the quenching one? Is it possible to couple a gas nitriding process to a qpq but only for the quenching-oxidising process?

Does there exist other similar HT with the same surface finishing (very important is uniformity and real black colour)? Thanks in a advance for any help.

L. Gessi
- Opera (MI) Italy


.

Kolene offers the qpq process and has put a paper about it on-line here.

 
Ted Mooney, P.E. - finishing.com Inc. - Brick, NJ


++

Dear sir,

I research about plasma nitrocarburizing post oxidation. Please help me about this subject.

Sincerely yours,

Mahdi Mirjani
Iranian surface research and engineering centre - Isfahan, Iran


Dear Reader: please choose what you want to do.

I want to post a question or inquiry of my own.
 
I want to answer or follow-up on this question publicly (in non-commercial fashion).
 
I am a supporting advertiser and want to reach the inquirer privately.





     

 Save This Page (why?)    -    Home    -    ©1995-2008 finishing.com