Letter 5076

Dilute Chromate 

.

Alright, this is a good one!

We make aircraft wings, and I have a problem with what I think to be the dilute Chromate sealant, first all wing parts go through anodizing and in the end they are dipped into the dilute chromate to act as a sealant (we no longer use the hot water seal, from there they are passed along to paint shop where they are masked. This is where the problem comes out, where the masking tape was directly on the wing skin, a yellowish color is left behind, which Im pretty sure is dilute chromate, but like I said its only where the tape was applied, where the paper was put at use its alright.

Am I missing a process somewhere, should pieces be air-forced dried before masking? should pieces be shower rinsed after the chromate application??

I also noticed that this problem is causing me adhesion problems!!! If anyone knows this one, let me know on somekind of test, cuz I went through plenty of testing and Im stumped on this one.

Terrence Double
- Momtreal,Quebec,Canada


Dear Reader, please --

Post a question on a different subject.
 
Answer or follow-up on this subject (in non-commercial fashion).
 

 


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com