You just missed the last thread on this, Dave. See letter 4369.
|
|
|
Stags-I used to buy them from JPS in Cincinnatti,OH. Kocour used to sell them also. Rings-I made my own from 316 SS weld wire, tig welded and polished. Calibrated them in the lab using a Stag. Had a set from 1" to 5".
Also remember using a ring after converting to SNAP-A/M. Ever see nickel plate look like corn flakes on a part. The extreme gross excess of A/M made the plate off the scale on a contractometer test. For the newer folks, the moral is the anti foamer in A/M prevents you from using the ring test.