Is there a chemical way of removing powder coating from brass without harming the brass in anyway? Is sandblasting absolutely necessary for good adhesion of powder coating to brass?
Kik, Shian Jer- Germany
.
If the powder is polyester or epoxy-polyester a cold solvent stripper made from Benzyl alcohol and containing 10 g/l KOH will remove it in about 30 mins without harm. Rinse off with water, but DO NOT add water to the product. R
Roger Bridger- Croydon, UK