Some clearcoating solutions pointer     

.

I am looking for product information and tips as to what to use and how to strip clearcoat off Aluminum running boards and what to use to polish and renew....... all info greatly appreciated, Stephen

Stephen Pond
autobody - Canada


September 30, 2008

Hi, Stephen. letter 11239 suggests that it can be removed with MEK / methyl ethyl ketone [linked by editor to product info at Amazon]. However, there are different clearcoat formulations and technologies, so that's not a guarantee that MEK / methyl ethyl ketone [linked by editor to product info at Amazon] would work for you, nor that it is practical. The most likely stripper is aircraft stripper [linked by editor to product info at Amazon], but this is methylene chloride, and quite noxious, toxic stuff. Good luck.

Regards,

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey

Classic Car Restorer's Handbook


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search