Plating on a high chrome surface
June 20, 2008
We are in the pogo pin industry. Can we hard chrome a pure copper plate and then plate another layer of silver as we need a hard surface and yet to be able to have a high electricity flow ( Doing resistance testing on our pogo pin after a few thousand cycling). We experiencing high wear and tear on our current design plate (pure copper plated with Ni then Silver)
Mike TanElectronic - Singapore
June 23, 2008
Hi, Mike. I don't know if that is practical or not. But what is very practical is electroless nickel (also very hard surface) followed by silver.
Regards,
|
Ted Mooney, P.E. finishing.com Brick, New Jersey |