Dear friends, firstly, thank you for your time and good advice on the forum.
It is true that steel parts that are stripped of decorative chrome and then re-plated will tend to rust in areas where two parts,as with a spot welded lap joint, are in close contact ? Every plant that I have taken my parts to has told me that this is an unavoidable side effect from when the original chrome was stripped. Thanks for your replies.
hobbyist - Taipei Taiwan