Electro polishing for weld clean-up

June 17, 2008

We do in-house TIG welding on 304 SS, basically to join a 3/4" or 5/8" shaft with clevis which has various OD ranging from .71" to 1.25".
After welding the dis-coloration need to be removed and we use electropolishing, which works great for welded with low power input while on higher power input weldings the clean up is not acceptable.

Does any one has any idea what went wrong or better means of removing the dis-coloration?

Thanks a lot.

Keffelew Assefa
- Vancouver, BC, Canada





Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com