49059

Electro plating on exposed steel  

June 18, 2008

Hi,
I have an steel bracket for which an electro plating has been done as coating. I would like to know, for an exposed steel , how much is the min thickness of electro plating is required. Currently, an 20-25 micron thickness of electro plating has been done. can anybody advise me on this.
regards,

Sri Srilakshmi
structural engineer - Bangalore, India


June 18, 2008

Hi, Sri. Sorry, I don't understand. What metal is the steel plated with and why? This is a very substantial thickness if it's zinc plated but a minimal thickness for nickel plating. Are you sure it's electroplated rather than hot dip galvanized? If you are speaking of structural use outside, such as a bridge component, this thickness doesn't sound like much.

Regards,


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey





Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com