Nickel plated steel wire turns yellow
June 16, 2008
Sir,
i am plating nickel on steel and copper wire from last 2 years but in
rainy and moisture seasons my plated wires changes its colour to
yellow.Can any one suggest me to solve this problem.
Thanks.
regards,
Ashish Sachdeva
plating shop employee - Ambala, Haryana, India
June 19, 2008
Hi Ashish,
U are doing a flash Ni.plating.Will u be able to increase the
thickness!!.
Alternative- dry well and keep it in a moister free atmosphere and
transport it to the customer as soon as possible.
regards
|
|
T.K. Mohan
plating process supplier
Mumbai, India
|
June 23, 2008
Dear
Mr.Ashish you can do carbon batch teatment to your nickel bath and
try to control over Brighteners and additives(If using)
Vishal Duse
plating process supplier - Aurangabad, Maharashtra, India
June 24, 2008
Dear Sir,
please do batch carbon treatment and pack the carbon regularly
and tru to minimise the use of organic additives and brightners
Thanks
Vishal Duse
- Aurangabad, Maharashtra, India


 |