Ecoat paint over galvaneal material  

June 17, 2008

Our company supply siderails made of galvaneal material. We have to ecoat the finish parts. The problem is we can not approve 1000 hours of salt spray. The same ecoat line is approved for 1000 hours salt spray but with regular steel. Do we need to do anythink diferent in ecoat process for the galvaneal?

Renato Brighenti
Manager - Cruzeiro, SP, Brazil