HOME FAQs BOOKS JOBS: Help Wanted Suggestions you are here: Hotline/Forum => Letter 49030
Electro Chemical De-burring of Micro Surgical Knife
June 13, 2008
Sir
We are manufacturing Micro Surgical knives from AISI 420 grade stainless steel material. We like to remove the edge grinding burr by using electro chemical machining process. At present we do buffing. Kindly suggest suitable process with diagram and technical details. Then we can develop this process. Any further more information required by you please mail us.
Regards,
ENGINEER - MADURAI, TAMIL NADU, INDIA
June 17, 2008
Electrochemical deburring is a technology that evolved from electrochemical polishing. There are numerous patents on the subject and I am sure that one of the larger razor blade manufacturers such as Warner Lambert, Schick or Gillette may be willing to license some of their older technology to you for a suitable fee. Alternatively, you can develop and use your own process, based on electropolishing.

Trevor Crichton
R&D practical scientist The Pheasantries - Chesham, U.K.
June 19, 2008
Anybody why require licensing such technological process, contact us. See picture attached.