49027
Finish Conversion: Spark Eroded VDI3400
June 13, 2008
I have a European Spec that calls for a Spark Eroded VDI 3400 Ref.
33 Finish. I am trying to find a U.S. Spec that is an equivalent to
the VDI callout. I have looked through a Tenibac Catalog and found
one that looks close using a magnifying glass but I would like to be
a little more exact.
George Turner