Commercial letter stripping chemical

June 12, 2008

I am an owner operator that can no longer afford to lease a box trailer due to the increasing fuel costs and have had to purchase a used trailer, thatIi am going to have to remove the letters and paint it myself.

So I am trying to find out what checmical to use to strip the letters off the trailer?

thanks
mb

Shiree Bellamy
buyer - Lithonia, Georgia


June 13, 2008

Hi, Shiree. If the trailer is aluminum, try aircraft stripper [linked by editor to product info at Amazon] (methylene chloride); it's noxious stuff, you need personal protective equipment and very good ventilation.

Regards,

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search