49012
Conversion coating without painting
June 11, 2008
Can we use conversion coating without painting in wet
atmosphere?
for example on the gritting of platform.
Majid Shahrjerdi
- Iran
June 11, 2008
Hi, Majid. "Conversion coating" is a context-dependent term. It
can mean, among other things, phosphatizing of steel or chromating of
aluminum. Chromated aluminum does not require painting. However,
phosphatized steel without paint is rarely considered a suitable
coating.
Regards,
|
|

Ted Mooney, P.E.
finishing.com
Brick, New Jersey
|
June 12, 2008
My opinion is that a conversion coating is a little better than
nothing in a wet atmosphere and is not recommended for an area of
high wear like a scaffold as it will wear off rapidly.
James Watts
- Navarre, Florida


 |