49006

Is Zinc Plate with Sodium dichromate finish RoHS compliant?  

June 11, 2008

While doing Zinc plate with Sodium dichromate finish, is it RoHS compliant.

Sudhir Kulkarni
Designer - Bangalore, Karnataka, India


June 11, 2008

Hi, Sudhir. Dichromate is Cr2O7-2. The chromium is in hexavalent state and is forbidden by RoHS. However, RoHS-compliant "chromates" are widely available (I put "chromate" is quotes because they are called trivalent chromate but are not really "chromate" because that is chemically CrO4-2).

Regards,


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey





Legal disclaimer boilerplate button