48797

Material displacement of roller burnish [Texas] 

May 15, 2008

I have a high tensile austenitic stainless steel materia; can I do roller burnish for 2.874" Dia. bore to a 32 RMS finish, 0.001" - 0.002" diametrical material displacement?

YunHua Zhao
product designer - Houston, TX, USA


May 19, 2008

Short answer is yes. Almost any media can achieve that result; therefore, I'm not sure why you want to burnish part?

AF Kenton
Nova Finishing Systems Inc.

Huntingdon Valley, PA








 

 Save This Page (why?)    -    Home    -    ©1995-2008 finishing.com