48749
Water pipe cleaning solution
[China]
May 8, 2008
I am helping my friend in China to find a chemical to clean the
12" to 20" water pipe. The water source is from the local river or
ground water. Water is used in a steel manufactory for cooling
purpose. They are using some chemical solution, soak inside the pipe
for 24 hours to clean the deposit (or corrosion). These are the
limited info. I have.
Lynn Chou