Passivation of 304L stainless tank in the field. [Texas]May 8, 2008 I want to test and passivate a 304L tank in the field and have been told that I can hydro and passivate at the same time using 3% nitric acid. I'm confused at this point and want to make sure it's done right before putting into service. Any help would be appreciated. Dave Mosley
May 21, 2008 I don't know what all is required in doing a hydro test on a new
tank (surfactants or other additives) but I would question the
effectiveness of that low a dilution of Nitric for providing an
adequate passivation. Todd Turner
June 3, 2008 Todd is correct, a thickened "gel" version citric acid passivation
solution is commonly used for application like this.
June 26, 2008 we are hving nitic storage tanks for storing 60% nitric acid of capacity 3000M3. Moc of the tanks is SS304L. I am facing the problem of weld leakage. canyou suggest some good way to repair and long lasting weld joints and some type of quality assurance plan to accomplish the good joints. MADAN MOHAN GUPTA
![]() |
Save
This Page (why?) - Home - ©1995-2008 finishing.com