We are thinking to prepare a acid solution in a truck (used to transport HCL) with HCL and and inhibitor Rodine. I would like to know if rodine can affect the internal covering made of Plastic+fiberglass and resin Derakeni (CatBO411).

Roberto Villarroel
Chemical Eng. - LA /Brazil


May 12, 2008

Please define rodine. What is it?

Guillermo Marrufo
Monterrey, NL, Mexico


June 11, 2008

Hello,

I don't know why are adding RODINE (see note) to the HCL if your Truck Tank is already coated with plastic.
Rodine should be used for parts being inmersed into HCL solution.
Other way, RODINE wouldn't attack (in the case) your Resin (alcohol is about 12% diluted.

Jose Castellanos
NOTE
RODINE => http://www.telfordindustries.com.au/Uploads/Images/Rodine%20213.pdf

Jose Castellanos
- Minneapolis, MN, USA








 