48619
Procedure for polishing aluminum wheels
[Florida]
April 26, 2008
Hi
I intend to polish 100 Alloy Wheels per day as following images:
(Image of the wheel after leaving the mould, and not machined),
and I intend to polish the spokes only. The size of the wheel is
13x5"
what kind of polish do you suggest?
How long does it take for an experienced person to finish polish each
wheel
Is it possible to apply a polyester powder coating on the spokes
other polishing the spokes? How is adhesiveness?
What other kind of coating do you suggest to prevent oxidation of the
polish surface.
Daniel Sanchez
product designer - Florida
June 13, 2008
I would certainly be interested to know if and how you find out
how to polish a hundred wheels a day, without hiring a hundred people
to do one each. It depends on the surface you begin with. I hand sand
and polish aluminum wheels. It takes hours and hours to do it by
hand.
Good luck !
John
John Smith