Insulation coating for CRCA steel
[India]
April 25, 2008
Sir,
I would like to have the insulation coating on CRCA metal enclosure
for electronics application. I am considering using Powdercoating and
can anybody suggest is there any alternative coating method available
which gives insulation?
Regards,
Dinesh Kumar
Product designer - Bangalore, Karnataka, India
June 11, 2008
Hello DINESH,
INSULATION?
I guest you are talking about electrical insulation.
There is an alternative using resins. They are widely utilised on
insulating electrical components.
There are resines one component Oven curing) or two components
(autocatalized or oven).
Jose Castellanos
- Minneapolis, MN, USA
June 16, 2008
Hello Jose. thank you.
Yes. it is for 24VAC electrical insulation. My design calls for metal
enclosure which holds the PCB.
However, I am looking for a cost effective alternative to powder
coating on to this metal enclosure..
Dinesh Kumar
- Bangalore, Karnataka, India
July 9, 2008
Hello Mr Dinesh Kumar,
E- Coat is a reasonbly good insulating coating. It is used even for
transformer cores.
regards,
|
Khozema
Vahanwala
Automaxx
Bangalore, Karnataka, India
|
|


 |