How to prevent mirror polished steel from scratch? [Thailand] 

March 29, 2008

What should I coat my mirror-polished stainless (No.8) with? It scratches easily.
I read some about Teflon coating. Is it good? What is the cost?
What is other choices?

Theera Sunthorn
businessman - Thailand


April 22, 2008

Nickel+chrome might be an option. Alternatively Electroless Nickel though more expensive will cover the surface uniformly if geometry is complex.

Guillermo Marrufo
Monterrey, NL, Mexico