Passivate stainless medical instruments
before or after TiN coatings?
March 4, 2008
Should we passivate before or after TiN coating on 17-4 ph
stainless steel.
I beleiee we should passivate before but I'm not totally sure.
Thanks for your help.
Scott Jones
- Mcmurray, PA, USA
March 6, 2008
Passivation should be before, since TiN is very corrosion
resistant by itself. It is quite thin, so it does not have an
infinite corrosion resistance life.
James Watts
- Navarre, Florida


 |