Fan nozzles versus cone for resist stripper [Georgia] 

March 5, 2008

Trying to find out which nozzle works best in stripping Dupont MM550 photo resist in a chemcut 547xli stripper. We're using Amino ethnol with choline stripper.

Ken McKinley
circuit board mfg - Robins, Georgia, U.S.


March 6, 2008

Hi Ken,

Use PVDF Jets ... available from BEX ... wide angle solid cone.

Freeman Newton
- White Rock, B.C. Canada