Nickel anodes for Nickel free plating?

March 3, 2008

As we are in the jewelry industries some European country's request for nickel free plating, We got down nickel free plating chemical from a reputed establishment.The inquiry is they told us to use nickel anode that really worries us because its back again nickel in the bath.Please educate me on this.

Mohamed Nuwais
Employee - Sri Lanka


March 5, 2008

Your concern is totally valid. You should not use nickel anodes. Perhaps neither their solution until you know exactly what they sold to you. G. Marrufo-Mexico

Guillermo Marrufo
Monterrey, NL, Mexico


March 7, 2008

Hi There,

Check with the supplier whether they gave you white bronze, or Palladium bath, there is no question of using Nickel Anode, it has to be Graphite or Carbon insoluble anodes.
Regards,

Praveen Kumar
    plating process supplier
Mumbai, India





Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com