Fixing crater problem in paint due to
defoamer
March 3, 2008
Dear
we found whenever add exta defoamer, paint will face crator problems;
so what we should do to re-condition it.
Aphichartd Dankul
production specialist in paint factory - Thailand
March 14, 2008
The defoamer you are using is probably a silicone based product.
Minute particles of silicone will float a very long way in the air
and contaminate paint, the metal to be coated, air-lines etc. Try
another type of defoamer, oil based or ask your supplier to give you
a less aggressive silicone based product.


 |