yikes...put in ceramic floors and moved stainless steel stove and dishwasher back in place......had to acid wash tiles and some splashed on appliances and marked them...anyway to cover/remove this?......then , son, waxed floors(even tho I said not to), and there is floor wax on appliances , too! eecchh....help! Christina.(I know ,I know, I should've covered the appliances but I didn't so help me anyway, ok?) thanks!

Christina Simmons
homeowner - Buffalo, New York


March 5, 2008

Dear Christina, No Worries. Scratch-B-Gone listed above will remove the chemical discoloration due to the acid splash. Use Acetone [link is to product info at Rockler] or perhaps rubbing alcohol to remove waxes first to exposed clean surface. Remember to think Scratch-B-Gone for your scratches and for heat scorching on your BBQ too! All the best.

Barry Feinman
Restore It Yourself, Inc

Carlsbad, California





Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com