How to do vinyl coating?
+++++++I shall want to do vinyl coating into a lead ball weight up to 2.5kgs.How shall I do this?I am a Indian . Please send me the details process.
Arindam Dutt- Kolkata, India
June 20, 2008
Hi, Arindam. What you are looking to do is sometimes called "plastisol dipping".
In broad terms the process includes cleaning the parts, applying a glue-like prime coat, dipping into the liquid plastisol tank, and finally, oven curing.
But it is possible that you might be interested in thermoplastic powder coating as an alternate. That process would be similar except instead of dipping the parts into the liquid plastisol you would dip them into a fluidized bed of thermoplastic powder like nylon or teflon. Good luck.