What coating protects stainless steel from
sulphuric acid?
+++++++
Our customer has stainless steel tubes that are used to process
waste water and treat human waste. They will be subject to sulphuric
acid and other corrosives. What can I coat the stainless steel tubes
with to protect them?
Jonathan Searle
Paint Shop Manager - Santee, California, USA
+++++++
Teflon or plastisol should do it. I rather doubt that a paint or
thermoset powder will be impervious enough. Good luck.
|
|

Ted Mooney, P.E.
finishing.com
Brick, New Jersey
|


 |