47039

How to get a good finish on brass wire and pipe  

+++++++

I am the quality Manager in company produce copper wires and pipes (brasses ) we use dichromate washing for good surface finishing after treatment with suphuric acid 10 %

we have unshining surface and some spots.

please help us

Nagyelgendy
production - Cairo, Helwan, Egypt


+++++++

Perhaps you can get a local process supplier in to look at your operation, Nagyelgendy, but I don't think you will get a shining surface without a bright dip step. Usually these involve nitric acid, although on a smaller scale or with cleaner work you might be able to use stabilized hydrogen peroxide in your sulfuric acid to provide the required oxidizing power.


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey





Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com