I need information regarding the black
trivalent chrome
+++++++
We feel interested to run this process but in Mexico nobody know
about this. I need to know if is better run Chloride or sulphate
process and which is the best process for black chrome trivalent.
Gabriel Ramirez
POP line - Guadalajara, Mexico
+++++++
Hello
U can go for chloride process i.e Acid Zinc and on it u can do Black
Triv pass. It gives very good results. All u have to do is that it
requires some extra care.
Hope it will help!
Sean Aarchr
- Chandigarh
+++++++
Well, that's like asking is red or green "better." It's a matter
of personal preference and experience. I use a chloride based
trivalent chrome and we experience very few problems as long as we
keep parts out of the bottom of the tank and we control our
temperature closely. I have never used sulfate based trivalent chrome
but I am sure there are relative advantages to each. In a situation
like this, ask your current proprietary chemical supplier about the
relative advantages of each, make some plant visits and make your
determination from there.
Daryl Spindler
- Nashville, TN, USA


 |