Can't achieve bright silver plating

+++++++

I am working at a fashion jewelery manufacturing co. I presently plate silver which becomes very dull and I have to polish it to get the bright finish. this takes a lot of time. maybe sombody can help me

M Nuwais

Mohamed Nuwais
Plating shop employee - Sri Lanka


+++++++

Mohammed,
Kindly ref.some of the posting such as Letter.No.46293.
u may get lot of information.Please give more detailes about what u do.
Regards

T.K. Mohan
    plating process supplier 
Mumbai, India


+++++++

Mohamed,
As T.K. noted, we have to have more info regarding your plating process. What is the substrate metal or underplate? Current density, bath analysis, deposit thickness, silver bath type, etc.

Mark Baker
Process Engineer - Syracuse, New York


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search