Can stainless 303 be hard chromed?
Hard Chrome |
|
I want to hard chrome stainless 303.
Can it be done and if so are there any special considerations?
Hobbyist - Flower Mound, Texas
+++++++
Yes, it can be hard chromed, R.C. It may require a different etch, but there would be no special considerations for an end user like yourself.
|
Ted Mooney, P.E. finishing.com Brick, New Jersey |