Hello All!

I m running a Rack plating tank of capacity 800 ltrs. of Acid Zinc.I m maintaining Metal as 35 gm/ltr. (30--35 gm/ltr.);Chloride as 130gm/ltr.(120--140 gm/ltr) & Boric as 33 gm/ltr.(30--35 gm/ltr.)
My problem is that i m facing the problem of HCD area i.e when I did Hull-Cell at 1 Amp. for 5 Mins. I have no Problem ,but when i did at 1 Amp. and for 10 Mins. a dark brown colored start appearing at HCD and after HNo3 dip I found dark Silver grey color in only HCD area whereas my LCD area and Medium area is cleared and shiny.So, what is that dark brown color.
Is it due to some Metalonic Impurities or what?
I have packed Zinc dust,Carbon at 100gm. twice
I have packed packed KmNo4 at 100gm.twice in order that no iron or any other impurity should be there.
I did Hull Cell at 1 Amp. at 10 mins. with only 'M' as there may be un-balanced M-R ratio, so what i find that in Hull-Cell of 250 ml. I put total 18.5 ml after various trial.So corresponding to 800 ltrs. it comes out to be 60 Ltrs. So should I go for it or not. Pls Tell.

Sean Aarchr
Engineer Q.A - Chandigarh


+++++++

The Indian brightners are not formulated to work at that metal concentration.

Reduce metal to 20 - 22 gms and Boric likewise. Reduce the chlorides to a 1 : 5 ratio to the metal and start work.

Khozema Vahanwala
Saify Ind
 
Bangalore, Karnataka, India


+++++++

Dear Khozema Vahanwala

I have also did the same thing for atleast 1 week. But in vail.

Sean Aarchr
- Chandigarh





Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com