Dear sir,

I am M.Sc Physics student from india and I am working in the field of metalic coatings by thermal evaporation methods but I want to know how we can do a metalic coating or a conductive coating onto non metalic (means non conductive) substrate? So, please suggest the relevant method and broadly. I am waiting for you answer.

Your's faithfully

Sudhir Bhatt
student - ahmedabad,gujarat,india


+++++++

Hello, Sudjir. I understood your introduction of yourself and I understood your question, but I'm not sure if I understood the relationship between the two well enough that my answer will be helpful -- but we have an FAQ on Metalizing Non-conductors that may be helpful.

I think you may be thinking of vacuum metalization with aluminum, though. This involves coating the substrate with a basecoat, then applying a very thin layer of aluminum by vacuum metallization, then appying a clear organic topcoat to protect it.

I think Ionedge or Vergason Technology could offer information and equipment. Good luck.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search